EN
In the work tests of the influence of the technological conditions on the basic applied properties of the Pb(Fe_{0.5}Nb_{0.5})O_3 ceramics were carried out. The Pb(Fe_{0.5}Nb_{0.5})O_3 specimens were obtained by a two-stage method of synthesizing (the niobite method), a technique of the powder mixture calcinations, changing a temperature range of the iron-niobate (FeNbO_{4}), whereas compacting was conducted by free sintering.