Metal-carbon composites have shown considerable hydrogen storage potential at room temperature. In the present work the behaviour of two different Pd amalgam doped carbon substrates, namely a carbogenic foam and a mildly oxidised ordered mesoporous carbon, are compared on the basis of their hydrogen sorption properties at 77 and 298 K and low pressures, aiming to investigate the effect of surface on the storage capacity. In both cases, the introduction of alloy nanoparticles leads to an improvement of the hydrogen uptake with respect to pure carbons. This effect is significant for the carbogenic foam however small for the ordered carbon. [...]
EN
Layered compounds with CdS particles supported on the ion-exchanger, γ-titanium dihydrogen phosphate, were prepared by the stepwise reaction of the ion-exchanger and cadmium solution, followed by reaction with H2S gas. The CdS content on the ion-exchanger is dependent on the timeframe of the H2S gas flow. The materials obtained were layered, as shown by the X-ray measurements that exhibit both precursor and CdS diffraction peaks. The thermal treatment of the material obtained gives evidence of its stability (≤ 320°C) before the CdS decomposition, which occurs in a single step. [...]
EN
Magnesium-based composites of 75 wt% Mg - (10, 15, 20) wt% Mg2Ni0.7Co0.3 - (15, 10, 5) wt% C mechanically activated for 30 min under argon in a planetary mill, were obtained. Their absorption-desorption characteristics were investigated under a pressure P = 1 MPa and temperatures of 623, 573, 473, 423 and 373 K. Desorption was carried out at 623 K and 573 K and a pressure of 0.15 MPa. All the three composites showed improved hydriding kinetics as compared to pure magnesium. However, the desorption temperature was somewhat higher than needed for practical application. [...]