Skip to main menu
Scroll to content
PL
|
EN
Full-text resources of PSJD and other databases are now available in the new Library of Science.
Visit
https://bibliotekanauki.pl
Search
Browse
About
test
Refine search results
Journals
1
Archives of Metallurgy and Materials
Years
1
2021
Authors
1
Kierat M.
1
Migas D.
1
Moskal G.
Preferences
Polski
English
Language
enabled
[disable]
Abstract
10
20
50
100
Number of results
Results found: 1
Number of results on page
10
20
50
100
Page
/ 1
Search results
Search:
in the keywords: Co-Ni superalloy
Sort By:
accuracy
title
date descending
date ascending
journal title
author
Limit search:
in any field
in the title of publication
in the title of journal
among author
in the keywords
in references
Page
/ 1
1
Full text local access
The Oxide Scales Formed on Different Co-Ni Based Superalloys During Isothermal Oxidation at 800 and 900°C
100%
Migas D.
,
Kierat M.
,
Moskal G.
,
Migas D.
,
Kierat M.
,
Moskal G.
Archives of Metallurgy and Materials
|
2021
|
vol.
66
|
issue
1
Page
/ 1
JavaScript is turned off in your web browser. Turn it on to take full advantage of this site, then refresh the page.