Micro-Abrasion Wear Behavior of Thermal-Spray-Coated Steel Tooth Drill Bits

Authors

Content

Title variants

Languages of publication

EN

Abstracts

EN
Wear behavior of four kinds of thermally sprayed coatings on steel tooth drill bits have been investigated by micro-abrasion wear test. The fixed ball micro abrasion wear test was applied for bare substrate and for thermal sprayed substrate of each sample. SiC and Al₂O₃ abrasive powders with grain size of 5 μm were used in the abrasion experiments. Ball rotational speed values of 140 rpm and applied loads of 1, 2 and 3 N were used. Experimental results show that the wear mechanisms of the coatings are micro-grooving and micro-rolling. Application of the coatings was found to have an influence on the wear mechanism of the samples. The results also indicate that wear resistance of thermally sprayed coatings can be correlated to porosity, hardness, plasticity, toughness, and cohesion properties of the coatings. In addition, wear resistance of the coated samples had increased in accordance with the increasing coating thickness.

Keywords

EN

Contributors

author
  • Iskenderun Tech. Univ., Faculty of Technology, Materials Engineering Department, Hatay, Turkey

References

  • [1] P.X. Moore, Drilling Practices Manual, 2nd ed., PennWell Publishing Company Oklahoma, USA 1986, p. 363
  • [2] R.E. Grimes, E.C. Felderhoff, H. Brown, Oil Gas J. 18, 76 (1992), doi: 10.1016/0148-9062(92)91878-9
  • [3] R.A. Bobo, J. Petr. Tech. 20, 700 (1968), doi: 10.2118/1843-PA
  • [4] K.W. Cummins, Technical Report No 28, Michigan State Univ. Inst. of Water Research, 1973
  • [5] D. Praillet, World Mining Equipments Sept., 20 (1998)
  • [6] K. Teii, T. Hori, S. Matsumoto, Thin Solid Films 519, 1817 (2011), doi: 10.1016/j.tsf.2010.10.017
  • [7] I. Mrochek, R. Gunzel, W. Matz, W. Moller, V. Anishchik, Nukleonika 44, 217 (1999)
  • [8] L.D. Yu, G.W. Shuy, T. Vilaithong, Surf. Coat. Technol. 128-129, 404 (2000), doi: 10.1016/S0257-8972(00)00642-3
  • [9] A. Kolitsch, E. Richter, Cryst. Res. Technol. 18, 5 (1983), doi: 10.1002/crat.2170180122
  • [10] M.J. Kupczyk, P. Siwak, J. ASTM Int. 8, 1 (2011)
  • [11] N.J. Kar, IADUSPE Drilling Conj., 1990, p. 49, doi: 10.2118/19910-MS
  • [12] M.W. Richert, B. Mikułowski, P. Pałka, A. Hotloś, M. Perek-Nowak, J. Surf. Eng. Mat. Adv. Techn. 3, 1 (2013), doi: 10.4236/jsemat.2013.31001
  • [13] P. Fauchais, A. Vardelle, in: Advanced Plasma Spray Applications, Ed. H. Jazi, InTech, 2012, doi: 10.5772/34448
  • [14] A.C. Karaoglanli, Sci. Adv. Mater. 7, 173 (2015), doi: 10.1166/sam.2015.2099
  • [15] A.C. Karaoglanli, B. Demirel, A. Turk, R. Varol, K.M. Doleker, Appl. Surf. Sci. 354, 314 (2015), doi: 10.1016/j.apsusc.2015.06.113
  • [16] R.I. Trezona, D.N. Alsopp, I.M. Hutchings, Wear 225, 205 (1999), doi: 10.1016/S0043-1648(98)00358-5
  • [17] M.M. Stack, M. Mathew, Wear 255, 14 (2003), doi: 10.1016/S0043-1648(03)00204-7
  • [18] M.M. Stack, H. Jawan, M.T. Mathew, Tribol. Int. 9, 848 (2005), doi: 10.1016/j.triboint.2005.02.013
  • [19] M.M. Stack, M. Mathew, C. Hodge, Electrochim. Acta 56, 8249 (2011), doi: 10.1016/j.electacta.2011.06.064
  • [20] A.C. Karaoglanli, Materials Technol. 49, 253 (2015)
  • [21] A. Kassman, S. Jacobson, S. Erickson, P. Olsson, M. Hedenqvist, Surf. Coat. Technol. 50, 75 (1991), doi: 10.1016/0257-8972(91)90196-4
  • [22] X.Z. Ding, C.T. Bui, X.T. Zeng, Surf. Coat. Technol. 203, 680 (2008), doi: 10.1016/j.surfcoat.2008.08.019
  • [23] A. Günen, M.S. Gök, A. Erdoğan, B. Kurt, N. Orhan, Tribol. Trans. 56, 400 (2013), doi: 10.1080/10402004.2012.756566
  • [24] K.T. Kembaiyan, K. Keshavan, Wear 186-187, 487 (1995), doi: 10.1016/0043-1648(95)07142-3
  • [25] G. Bolelli, L. Lusvarghi, R. Giovanardi, Surf. Coat. Tech. 202, 4793 (2008), doi: 10.1016/j.surfcoat.2008.04.056
  • [26] R. Pileggi, M.M. Tului, D. Stocchi, S. Lionetti, Surf. Coat. Tech. 268, 247 (2015), doi: 10.1016/j.surfcoat.2014.10.007
  • [27] D.A. Stewart, P.H. Shipway, D.G. McCartney, Acta Mater. 48, 1593 (2000)
  • [28] J.K.N. Murthy, B. Venkataraman, Surf. Coat. Tech. 200, 642 (2006), doi: 10.1016/j.surfcoat.2004.10.136
  • [29] P. Vuoristo, K. Niemi, A. Makela, T. Mantyla, Proc. 7th National Thermal Spray Conference, Boston, Massachusetts, 1994, p. 121
  • [30] A. Karimi, Ch. Verdon, Surf. Coat. Tech. 57, 81 (1993)
  • [31] H. Sin, N. Saka, P. Suh, Wear 55, 163 (1979), doi: 10.1016/0043-1648(79)90188-1
  • [32] D.L. Duan, S. Li, X.H. Duan, Z.S. Li, Tribol. Trans. 48, 45 (2005), doi: 10.1080/05698190590896915
  • [33] M.S. Gok, Y. Kucuk, V. Koc, O. Gencel, W. Brostow, Mech. Adv. Mater. Struc. 18, 389 (2011), doi: 10.1080/15376494.2011.563413
  • [34] K.I. Schiffmann, R. Bethke, N. Kristen, Surf. Coat. Techn. 200, 2348 (2005), doi: 10.1016/j.surfcoat.2005.01.015
  • [35] I.M. Hutchings, Tribol. Intern. 31, 5 (1998), doi: 10.1016/S0301-679X(98)00004-8
  • [36] ASTM G77-05 Standard Test Method for Ranking Resistance of Materials to Sliding Wear Using Block-on-Ring Wear Test (2010)

Document Type

Publication order reference

Identifiers

YADDA identifier

bwmeta1.element.bwnjournal-article-appv130n1056kz
JavaScript is turned off in your web browser. Turn it on to take full advantage of this site, then refresh the page.