Origin of Imperfections in ⟨100⟩ SrLaAlO_{4} Crystals

Content
Title variants
Languages of publication
EN
Abstracts
EN
In Czochralski-grown SrLaAlO_{4} crystals with ⟨100⟩ orientation, (001) planar faults extending through the entire crystal boule can frequently be observed. Chemical etching and transmission electron microscopy including energy dispersive X-ray spectroscopy were used to characterise their nucleation sites, these being located in the upper part of the crystal cone. Three serious sources were found: (1) lateral {001} facets, (2) grown-in defects in the seed, and (3) small particles of a second phase in the interior of the cone. These particles were identified as trigonal and cubic form of lanthanum oxide with a different Sr content.
Keywords
EN
Year
Volume
92
Issue
1
Pages
157-162
Physical description
Dates
published
1997-07
References
Document Type
Publication order reference
YADDA identifier
bwmeta1.element.bwnjournal-article-appv92z117kz
Identifiers
JavaScript is turned off in your web browser. Turn it on to take full advantage of this site, then refresh the page.