A stable superhydrophobic surface of stearic acid grafted zinc was fabricated with two steps, that is, the zinc surface was firstly treated with glow discharge electrolysis plasma (GDEP) and then followed by a grafted reaction of stearic acid onto the treated zinc surface. Results indicated that the wettability of zinc substrate changed from superhydrophily to superhyphodrobicity with a water contact angle (CA) up to 158° and a water sliding angle (SA) less than 5°. The surface morphology and composition were characterized by scanning electron microscopy (SEM) and X-ray diffraction (XRD), respectively. [...]
Publisher

Journal
Year
Volume
10
Issue
6
Pages
1766-1772
Physical description
Dates
published
1 - 12 - 2012
online
21 - 9 - 2012
Contributors
author
  • Chemistry & Chemical Engineering College, Northwest Normal University, Lanzhou, 730070, P. R. China, jzgao@nwnu.edu.cn
author
  • Chemistry & Chemical Engineering College, Northwest Normal University, Lanzhou, 730070, P. R. China
author
  • Chemistry & Chemical Engineering College, Northwest Normal University, Lanzhou, 730070, P. R. China
author
  • Chemistry & Chemical Engineering College, Northwest Normal University, Lanzhou, 730070, P. R. China
author
  • Chemistry & Chemical Engineering College, Northwest Normal University, Lanzhou, 730070, P. R. China
References
  • [1] J.M. Xi, F. Lin, L. Jiang, Appl. Phys. Lett. 92, 053102 (2008) http://dx.doi.org/10.1063/1.2839403[Crossref]
  • [2] Z.G. Guo, W.M. Liu, B.L. Su, Appl. Phys. Lett. 92, 063104 (2008) http://dx.doi.org/10.1063/1.2841666[Crossref]
  • [3] M. Li, J. Zhai, H. Liu, Y.L. Song, L. Jiang, D.B. Zhu, J. Phys. Chem. B 107, 9954 (2003) http://dx.doi.org/10.1021/jp035562u[Crossref]
  • [4] X. Hong, X.F. Gao, L. Jiang, J. Am. Chem. Soc. 129, 1478 (2007) http://dx.doi.org/10.1021/ja065537c[Crossref]
  • [5] G.X. Li, B. Wang, Y. Liu, T. Tan, X.M. Song, H. Yan, Appl. Surf. Sci. 255, 3112 (2008) http://dx.doi.org/10.1016/j.apsusc.2008.08.107[Crossref]
  • [6] C.S. Liu, Z.W. Li, L. Wang, Z. Xu, Key Eng. Mater. 368, 1374 (2008) http://dx.doi.org/10.4028/www.scientific.net/KEM.368-372.1374[Crossref]
  • [7] K.K.S. Lau, J. Bico, K.B.K. Teo, M. Chhowalla, G.A.J. Amaratunga, W.I. Milne, G.H. McKinley, K.K. Gleason, Nano Let. 3, 1701 (2003) http://dx.doi.org/10.1021/nl034704t[Crossref]
  • [8] W. C. Wu, M. Chen, S. Liang, X.L. Wang, J.M. Chen, F. Zhou, J. Colloid Interface Sc. 326, 478 (2008) http://dx.doi.org/10.1016/j.jcis.2008.06.041[Crossref]
  • [9] E. Bormashenko, Colloids Surf. A 324, 47 (2008) http://dx.doi.org/10.1016/j.colsurfa.2008.03.025[Crossref]
  • [10] L. Feng, S. Li, Y. Li, H. Li, L. Zhang, J. Zhai, Y. Song, B. Liu, L. Jiang, D. Zhu, AdV. Mater. 14, 1857 (2002) http://dx.doi.org/10.1002/adma.200290020[Crossref]
  • [11] B.T. Qian, Z.Q. Shen, Langmuir 21, 9007 (2005) http://dx.doi.org/10.1021/la051308c[Crossref]
  • [12] M.L. Ma, Y. Mao, M. Gupta, K.K. Gleason, G.C. Rutledge, Macromolecules 38, 9742 (2005) http://dx.doi.org/10.1021/ma0511189[Crossref]
  • [13] X. Zhang, F. Shi, X. Yu, H. Liu, Y. Fu, Z.Q. Wang, L. Jiang, X.Y. Li, J. Am. Chem. Soc. 126, 3064 (2004) http://dx.doi.org/10.1021/ja0398722[Crossref]
  • [14] F. Shi, X.X. Chen, L.Y. Wang, J. Niu, J.H. Yu, Z.Q. Wang, X. Zhang, Chem. Mater. 17, 6177 (2005) http://dx.doi.org/10.1021/cm051453b[Crossref]
  • [15] B. Xu, Z.S. Cai, Appl. Surf. Sci. 254, 5899 (2008) http://dx.doi.org/10.1016/j.apsusc.2008.03.160[Crossref]
  • [16] J.P. Youngblood, T.J. McCarthy, Macromolecules 32, 6800 (1999) http://dx.doi.org/10.1021/ma9903456[Crossref]
  • [17] L. Zhai, F.Ç. Cebeci, R.E. Cohen, M.F. Rubner, Nano Lett. 4, 1349 (2004) http://dx.doi.org/10.1021/nl049463j[Crossref]
  • [18] X.Y. Ling, I.Y. Phang, G.J. Vancso, J. Huskens, D.N. Reinhoudt, Langmuir 25, 3260 (2009) http://dx.doi.org/10.1021/la8040715[Crossref]
  • [19] T. Nishino, M. Meguro, K. Nakamae, M. Matsushita, Y. Ueda, Langmuir 15, 4321 (1999) http://dx.doi.org/10.1021/la981727s[Crossref]
  • [20] H. Yabu, M. Takebayashi, M. Tanaka, M. Shimomura, Langmuir 21, 3235 (2005) http://dx.doi.org/10.1021/la050013w[Crossref]
  • [21] J.Z. Gao, A.X. Wang, Y. Fu, J.L. Wu, D.P. Ma, X. Guo, Y. Li, W. Yang, Plasma Sci. Technol. 10, 30 (2008) http://dx.doi.org/10.1088/1009-0630/10/1/07[Crossref]
  • [22] R. Joshi, R.D. Schulze, A.M. Plath, J.F. Friedrich, Plasma Proc. Polym. 5, 695 (2008) http://dx.doi.org/10.1002/ppap.200700175[Crossref]
  • [23] M.B.O. Riekerink, J.G.A. Terlingen, G.H.M. Engbers, J. Feijen, Langmuir 15, 4847 (1999) http://dx.doi.org/10.1021/la990020i[Crossref]
  • [24] D.S. Wavhal, E.R. Fisher, Langmuir 19, 79 (2003) http://dx.doi.org/10.1021/la020653o[Crossref]
  • [25] A.B.D. Cassie, S. Baxter, Trans. Faraday Soc. 40, 546 (1944) http://dx.doi.org/10.1039/tf9444000546[Crossref]
Document Type
Publication order reference
Identifiers
YADDA identifier
bwmeta1.element.-psjd-doi-10_2478_s11532-012-0116-0
JavaScript is turned off in your web browser. Turn it on to take full advantage of this site, then refresh the page.